Never done Rietveld on it, but check out:
V. Petkov, R. G. DiFrancesco, S. J. L. Billinge, M. Acharya and H. C.
Foley, Local structure of nanoporous carbons, Philos. Mag. B 79, 1519
(1999).
for a real-space refinement. I can send you a copy if you can't get
hold of it yourself.
Best regards,
S
ruggeri wrote:
Hello all,
Has anybody tried to refine turbostratic carbon with GSAS?
In the literature, the main peaks observed are the 002, 100, 004 and 110
lines.
If yes, what Pearson symbol is recommended for the refinement?
Regards.
--