Dear All,
I am trying to do quantitative analysis using GSAS. I have to analyze some
mixtures with a known fraction of one phase. How can I constrain in GSAS one
phase fraction (weight %) to a given value, in the meantime allowing the
remaining phase fractions to vary?
I have unsuccessfully been trying with various starting values of the phase
fraction, then switching off the refinement flag, but in the refinement the
phase fractions always converge to the (almost) same wt % values, different
(obviously, Murphy's?!) for the known phase from the expected value. Thanks
in advance for your kind attention.
Best Regards Natale Perchiazzi
§§§§§§§§§§§§§§§§§§§§§§§§§§§§§