At 09:19 PM 2/16/99 +0100, you wrote:
>>Sorry to bug people here again, but when I use REFLIST, I only get a list
>>of peak positions and Fcsq/FcTsq. Are these the calculated peak
>>intensities?
>>
>>Thank very much and in advance,
>>
>>Tao
>>2/5/99
>
>
>Did you get an answer from the GSAS community ? I noticed the same, the
>FOBS are missing from REFLIST.
>

You have to turn the FOBS flag in "least squares controls".