>> Could any of you point me to the good document about the method of applying
>> constraints in GSAS?
>> I am trying to figure out some complex cationic intermixing in a layered
>> cuprate superlatttice compound.
>> But I couldn't find a good documentation in the manual. Specially trouble
>> with a constraint with >2 variables.
>> For example, how do you make a constraint for something like x+2y+2z=1.
>> Thanks for your help.
>In a few words -- you probably can't do that with GSAS. This is not true
>of all Rietveld codes, but in GSAS a variable parameter can only appear
>in one constraint equation. One option that might help would be to put a
>soft constraint on the total composition.
>
Yes you can. You have to use a trick which is detailed in (J.-M. Joubert et
al., J. Appl. Crystalogr. 31 (1998) 327-332).
If you have three atoms on the same site and want to refine occupancy
factors (theoretically it is only possible if you have two data sets, for
example X-ray and neutrons), you have to introduce a fourth fictive atom :
You have, for example :
Atom 1, Ni, occupancy x
Atom 2, Mn, occupancy y
Atom 3, Co, occupancy z
and wants to constrain x+2y+2z=1
You introduce :
Atom 4, Ni, occupancy u
and change occupancy of atom 1 to v in such a way that u+v=x
Set the constraints on the parameters shifts :
du=-2dy
dv=-2dz
You will maintain by this way the condition u+v+2y+2z=x+2y+2z=1
Regards.
Jean-Marc Joubert
---------------------------------------------------------------
Jean-Marc Joubert
Laboratoire de Chimie Metallurgique des Terres Rares
CNRS - UPR 209
2-8 rue Henri DUNANT,
94320 THIAIS CEDEX - FRANCE
Phone: 33 (0)1 49 78 12 11
Fax: 33 (0)1 49 78 12 03
Email: [EMAIL PROTECTED]