On Tue, 5 Jan 1999 14:15:38 -0300 (GRNLNDST), Erica Goncalves Gravina - ig 
wrote:

>Hi every one!
>My name is Erica and I am a Chemistry student at the University of 
>Brasilia, Brazil. I am still doing my graduation and I've been working 
>with the refinement of minerals since 1996 but this year I started a new 
>project with polymers so, I decided as soon as possible do the refinement 
>of polymers structure.
>So talking to my tutor he said that is not commum a refinement of this 
>materials using the Rietveld method so what I would like to know from you 
>is some papers and works whith this subject that already exist.
>If someone can help me I will be very glad.
>Thank you
>Miss Gravina
>
>
>
>
>My e-mail : [EMAIL PROTECTED]
>

Hi Erica!

Peter Friedel has done (and still does) Rietveld refinements of polymers.
He works at the Institute for Polymer Research here in Dresden, Germany. 
Please, visit our BGMN home page at
  http://www.bgmn.de
You will find links to
-Peter Friedels pages explaining how our Rietveld Refinements of polymers
 work. Of course, Peter Friedel gives a list of his publications.
-my personal homepage, which includes a list of our actual publications.
 Some of them fit the area of polymers Rietveld refinement.

Good luck!

Joerg Bergmann