Any filler compound is going to add alot of weight, given what you 
describe...

Re-skin it...

On 2/13/2012 7:37 AM, robert gill wrote:
> Robert GillHi, I have a question about the best way to surface and level the 
> ply fuse skins aft of the cockpit area without adding to much weight, the 
> skins have bowed inward up to 3/8" in some ares particularly just under the 
> top stringer, should  I glass the skin first with deck cloth then use foam to 
> build the areas out then lay another layer of deck cloth over the areas that 
> have been leveled out, or put the foam straight on the ply skin then glass 
> over that, or glass the ply skin as before and just keep filling with micro 
> until the surfaces are flat and smooth ( how thick can you go with micro? ), 
> or does any one else have a better idea.                                      
>       
> _______________________________________
> Search the KRnet Archives at http://mylist.net/private/krnet/
> to UNsubscribe from KRnet, send a message to krnet-le...@mylist.net
> please see other KRnet info at http://www.krnet.org/info.html

Reply via email to