Robert GillHi, I have a question about the best way to surface and level the
ply fuse skins aft of the cockpit area without adding to much weight, the skins
have bowed inward up to 3/8" in some ares particularly just under the top
stringer, should I glass the skin first with deck cloth then use foam to build
the areas out then lay another layer of deck cloth over the areas that have
been leveled out, or put the foam straight on the ply skin then glass over
that, or glass the ply skin as before and just keep filling with micro until
the surfaces are flat and smooth ( how thick can you go with micro? ), or does
any one else have a better idea.