Some say use a layer of deck cloth, some, me, say NO way. No layer of resin needed if no glass. Just use s good filler primer. That is what I did and you cannot tell it is wood. You will have to fill and sand either way, so why add the work and weight.
Dan Heath On Sep 13, 2013, at 3:16 PM, Robert Boyd <iflyexp at gmail.com> wrote: > Is it necessary or common to cover the fuselage with a layer of glass? Or > just a coat of epoxy? I seem to be getting told a few different things buy > some guys in the area so I thought that I would put it out to all the > experts in the KR2 family. > Bob in Frazeysburg Ohio > _______________________________________________ > Search the KRnet Archives at http://tugantek.com/archmailv2-kr/search. > To UNsubscribe from KRnet, send a message to KRnet-leave at list.krnet.org > please see other KRnet info at http://www.krnet.org/info.html > see http://list.krnet.org/mailman/listinfo/krnet_list.krnet.org to change > options