On Sun, 2008-07-27 at 07:49 -0400, gene wrote:

> have you guys seen the 'tin-whisker' problem with lead free solder?
> 
> 
> _______________________________________________
> geda-user mailing list
> [email protected]
> http://www.seul.org/cgi-bin/mailman/listinfo/geda-user


Tin whiskers are a massive problem in my line of work and we spend an
awful lot of
time and money investigating its causes and developing mitigation
strategies. We 
are looking to get 25+ years from our devices so it is something that
has to be actively
addressed. For now it seems we are not able to use 100% Matte Tin. 

If you need any information on it then let me know and I can do some
digging to get
the latest spin.

Best regards

Sandy