The other day, I noted the 1993 replication of
Mills is available on the net, here:
http://hydrino.org/documents/final-report-nascent-hydrogen.pdf
There is another quality replication of the Mills effect, in this paper:
Mengoli, G., et al., Anomalous heat effects
correlated with electrochemical hydriding of
nickel. Nuovo Cimento Soc. Ital. Fis. A, 1998. 20 D: p. 331.
Unfortunately, I cannot get permission to upload
this one. Let me quote the Summary and some of
the Introduction, which describes some of the history of the claim:
Summary. The hydrogen evolution reaction at
sintered nickel in H2O-K2CO3 electrolyte was
investigated by electrochemical and calorimetric
techniques. Hydrogen evolution was accomplished
with surface conversion of Ni into fl-Ni-hydride,
the extent of this reaction being strongly
enhanced by temperature. Isoperibolic or
isothermal calorimetry measurements show that
electrochemical hydriding, especially at a
temperature close to the boiling point of the
electrolyte, is paralleled by anomalous heat
evolution in large excess of electric power
input. Electrochemically activated Ni electrodes,
led in open circuit, keep on doing heat.
1. - Introduction
Although generation of excess energy by
electrolytic reduction of light water at either
nickel or other metal cathodes was claimed by
Fleischmann and Pons in their 1989 patent [1] it was subsequently not verified.
The first detailed study on the subject was that
published two years later by Mills and Kneizys
[2]. They found a power output several times
exceeding the Joule power input during
electrolysis with low current density of aqueous
K2CO3 at Ni plate electrodes: no anomalous
effects were observed with Na2CO3 electrolyte.
According to Mills, exotic physics were involved,
whereby hydrogen atoms shrink . . .
Noninsky, was the first to confirm Mills'
findings through reliable heat loss differential calorimetry [3].
In 1992, Bush published new data on the H2 0-Ni
system [4]. Excess heat was systematically observed . . .
At the ICCF IV meeting, Srinivasan et at [5]
independently reported both excess heat and
tritium generation during electrolytic reduction
of aqueous alkali solutions at the Ni cathode.
In 1993, two works were published on the subject.
The first, by Notoya [6] gave solid evidence of
the thermal phenomenon: not only was the power
output three times higher than the power input,
but this level was attained in a few hours, so
that calorimetric measurements were probably not
affected by the errors and/or artifacts which may
occur during long electrolyses. The above author
used a small (1.0 x 0.5 x 0.1 cm3) sintered Ni
cathode which sustained high current (0.5 A) with
remarkable specific power production (1 W/cm2).
Results were interpreted according to Bush's hypothesis.
The second work, by Ohmori and Enyo [7],
investigated other electrolytes (alkaline
sulfates and carbonates) and metal cathodes (Ag,
Au, Sn) in addition to the H2O/K2CO3 - Ni system:
anomalous heat effects were observed in most of
the systems excluding H2O/Na2 CO3-Ni and H2O/Li2 SO4-Ni.
In 1994 Mills et al. [8] and Mills and Good
(1995) [9] again published works on the
calorimetry of H2O reduction at Ni. Having
increased the scale of the original process,
greater excess power (41 W, eight times the I x V
total input power) was measured with K2CO3,
whereas negative results were again obtained with Nat CO3.
In 1994, Focardi, Piantelli and Habel [10]
reported that the interaction of subatmospheric
H2 (500-600 mBar) with Ni at temperatures of over
200°C gave rise to large enthalpy release.
Hydrogen was loaded into the Ni sample using
electromagnetic fields and temperature/pressure
perturbations: after a long period of induction
the system evolved into a state in which heat (>5
W/cm2) was emitted and was steadily self sustaining for months.
The above literature, although not exhaustive,
lists the most important contributions to this intriguing topic. . . .
- Jed