WHY use a glue gun ??
I drill holes in a thin wood slat,
drop the silver wires through the holes
and bend over the ends on top.
Smitty
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

On Tue, May 15, 2012 at 2:16 AM, Ode Coyote <[email protected]>wrote:

>
> Good morning Ode, I have been trying to POST this message, to [Silver
> List], but not showing-up! Suspect problem...maybe due to my posting
> URL/(address)...not being same as when I originally subscribed for Eskimo
> LIST sign-up... very long time ago? Post was Response to Sulfur
> CONTAMINATION posting, by Mike Monett and after you read what I'm trying to
> Technically present...think you may...concur? Feel FREE...to edit any text
> if you want to shorten message... is OK...by me. Since you are mentioned in
> my CS List posting, thought you might...forward? (Unlike
> Saint-Michael...Only Preach, when I have something Valid to SAY.;~) Thank
> you, Dok Dallas ========================================================
> Re: CS>Contamination, think Dok, found Source?
>  FROM:   * Dok Dallas
> TO:   * [email protected]
>    Monday, May 14, 2012 1:02 AM
>
>  Dear Mike, I have been brewing high ppm EIS at lower ION Drift-currents,
> for over 16 years and never saw any serious TRODE contamination in my Brew
> Cell...like Yours? Recently, Ode pointed out "NO Contamination, without
> Sulfur source", I agree~ So last Fall...I used my years of problem solving
> (pragmatic) SKILLS as MSEE, to start looking closely at everything you were
> doing in pictures...and soon, had good HUNCH....since you were only person,
> I ever saw waving HOT GLUE GUN to anchor new SILVER electrode(s), firmly to
> COROPLAST...located a Suspect!
> Also last year, in my one & only post to your silver-cell group, I offered
> you my long time proven working design solutions for ultra low-cost DIY
> BREW CELLS and was promptly placed on [MODERATION] after deleting, Doks
> (only) POST!
> The SULFUR CONTAMINATION is most likely coming from... the HOT GLUE, or
> perhaps also other (unknown) IONIC contaminates, found in COROPLAST?
> Did you ever consider what happens thermally to HOT GLUE, when Heated..?
>  While at elevated temperatures...it's bubbling out all kinds of,
> NASTY...IONS*
> If that weren't bad enough...MSDS for COROPLAST...is Decomposition RISK*
> http://en.wikipedia.org/wiki/Hot-melt_adhesive#Materials_used
> <[SULFUR]*
>