EDTA CIF

2013-11-03 Thread hd yahoo
Dear all, I'm looking for CIF of EDTA, I need it for reitveld calculation. Any one can help me. Regards, Dr. H.D. DRISS X-RAY and imaging unit. Post-doc: King Abdulaziz University. Djeddah KSA. ++ Please do NOT attach files to the whole

Re: Asymmetry peak shape difference between (pellet/powder)

2017-12-09 Thread hd yahoo
Le 12/9/2017 à 7:49 PM, N. Dragoe a écrit : Hi ZnO can also have a darker colour if it is obtained by thermal treatment in low pressure of oxygen. In my opinion, if all else is correct -I mean normal Soller slits, correct height,… etc- there might be sample strain. Regards N Le 9 déc. 2017

update my email

2017-12-09 Thread hd yahoo
Dear all, please update my email: Old email: hd_i...@yahoo.fr new email : hidr...@kau.edu.sa best regards, -- Dr. Hafedh DRISS X-Ray and Electron Microscopy Lab Department of Chemical and Materials Engineering Faculty of Engineering, King Abdulaziz University Jeddah, Kingdom of Saudi Arabia