Re: Asymmetry peak shape difference between (pellet/powder)

2017-12-09 Thread Nilesh Kulkarni
yes that is surprising. pellet is black while powder is white. ZnO pellet should also have been white. ​ -- With Regards, Nilesh Kulkarni. Tata Institute of Fundamental Research

Re: New Panalytical x-ray tubes ?

2018-02-07 Thread Nilesh Kulkarni
yes we have been using Empyrean tube with new HT cable for almost 2-3 years. ​ -- With Regards, Nilesh Kulkarni. Tata Institute of Fundamental Research Department of Condensed Matter