Dear All
I have some fixed wavelength X-ray diffraction data where the step size
in 2-theta is 0.015 degrees. It appears from the GSAS manual that the
step size must be in centidegrees - does this mean that I have to throw
away every other data point ?
Keith R.
Dear All
Sorry about the 'stupid' question - my problem was not that I couldn't
convert 0.015 degrees to 1.5 centidegrees - but I assumed that this had
to be as integer centidegrees in the data file !
Thanks for all the advice
Keith R
Sorry about the 'stupid' question - my problem was not that I couldn't
convert 0.015 degrees to 1.5 centidegrees - but I assumed that this had
to be as integer centidegrees in the data file !
Thanks for all the advice
Keith R
Dear All
Can anyone suggest a good, recent review of standards (reference
materials) used in X-ray diffraction.
Thanks in advance
Keith D. Rogers
Title: RE: Siemens D500
Armel - you might try HiltonBrookes in the U.K. (http://www.xrays.u-net.com/).
We also have an aging D500 - what particular spares are you looking for ?
Keith R.