Alternative suppplier for QPA standards

2024-08-15 Thread Jan Rohlíček
Dear All, SRM 676 (corundum for QPA) at NIST has been out of stock for some time. Is there an alternative supplier for some similar standard(s)? Thank you in advance, Jan Rohlicek Institute of Physics CAS Cukrovarnicka 10/112 162 00 Prague 6 Tel: (+420) 220 318 484 Email: rohli...@fzu.cz

Proposal call for SNS and HFIR closes August 28

2024-08-15 Thread Proffen, Thomas
Just a reminder - SNS and HFIR are currently accepting General User proposals for cycle 2025-A. The deadline is coming up on Wednesday, August 28. Proposals awarded beam time at SNS are projected to run January 28 to May 27, 2025. Details about instrument participation and conditions are provid

Re: Alternative suppplier for QPA standards

2024-08-15 Thread Matthew Rowles
Hi Jan Independent Minerals Standards have a corundum certified at 99.04% crystalline. It was done* via external standard calibration by reference to NIST 676a. https://imstandards.com.au/independent-mineral-standards-releases-ims135/ *I was involved in the XRD measurements that were used in th