Hi... try PowDLL from http://users.uoi.gr/nkourkou/
The software gives the opportunity to convert input
files to multiple formats.
Have in mind that this software requires .NET
framework installed.
Dr.N.Kourkoumelis
- Original Message -
From:
Liliana
Viciu
To: [EM
Dear Rietvelders,
Does anyone can provide the sources for purchasing XRD standards materials, such
as CeO2 and Y2O3?
I need few grams of these for calibration of our XRD.
Thank in advance.
regards
stephen
Dear Stephen,
I have prepared XPD-standard Y2O3 by firing Y2O3 (99.999) from Aldrich
at 1200 ºC for 72 hs. (as done in 41-1105 PDF card).
I would also like to ask the other list members if anyone has calibrated
the size-strain broadening of Y2O3 against LaB6, because I have no
access to LaB6 and I'
> Dear Stephen,
> I have prepared XPD-standard Y2O3 by firing Y2O3 (99.999) from Aldrich
> at 1200 ºC for 72 hs. (as done in 41-1105 PDF card).
> I would also like to ask the other list members if anyone has calibrated
> the size-strain broadening of Y2O3 against LaB6, because I have no
> access t
Dear collegues,
we intend to convert Seifert XRD files (njc). Is there a software tool
available for the 'fast' conversion of "njc" files to "rd" and / or
"raw" format without loosing information such as type of tube and so on?
Usually we use Ascii transformation but this includes too many step
Hi,
At 02:09 PM 12/7/2004 +, you wrote:
> Dear Stephen,
> I have prepared XPD-standard Y2O3 by firing Y2O3 (99.999) from Aldrich
> at 1200 ºC for 72 hs. (as done in 41-1105 PDF card).
> I would also like to ask the other list members if anyone has calibrated
> the size-strain broadening of Y2O3
Bruker will send you their program raw2rawg for
free on request. It works for converting their RAW files into GSAS files,
at least on my D5000 system.
- Kurt c
- Original Message -
From:
Liliana
Viciu
To: [EMAIL PROTECTED
Dear Kurt,
Please may have a copy too? Will that work for D500 data?
Regards
William
On Tue, 7 Dec 2004, Kurt Leinenweber wrote:
Bruker will send you their program raw2rawg for free on request. It works for
converting their RAW files into GSAS files, at least on my D5000 system.
Dear All,
Unfortunately, I can't supply the program myself. It came from Bruker (In
the US: 1-800-234-XRAY). As I said, they sent it to me for free and I don't
see why they wouldn't give it to anyone who wants it. Better yet, it might
be a newer version. I think it will work for D500 data too.
Apologies - I think I inadvertently posted my reply meant just for
Lachlan to the whole group!
Robin Shirley