Re: density of dislocations from the lattice microstrains

2004-04-07 Thread Radovan Cerny
Dear Angel L., the bible is: Krivoglaz, M. A. (1969). Theory of X-ray and Thermal Neutron Scattering by Real Crystals. New York: Plenum. and for useful formula you can have a look on some of the following publications (the list is definitely not complet): Wilkens, M. (1970). Phys. Status Solidi

Re: density of dislocations from the lattice microstrains

2004-04-07 Thread Andreas Leineweber
Dear Angel, there is a vast number of publications about this, and each one will give you a different formula. There is some physics behind the different methods, but it is not a straightforward procedure. Most methods rely, however, on the analysis of Fourier coefficients. Look at Kamminga&Delh

density of dislocations from the lattice microstrains

2004-04-07 Thread alortiz
Dear colleages, Could any of you give the details about the procedure (equations, methods) to deduce the density of dislocatins from the lattice microstrains obtained from the Stokes and Wilson or variance or integral breadth methods. Thanks in advance. Sinverely yours, Angel L.