Re: cubic lithium niobium oxide

2001-05-25 Thread Uwe Kolitsch
Flux growth and crystal structure determination of trilithium niobate Shishido et al. (1996) J. Alloys Compounds 234, 256-259 Li3NbO4 Ukei et al. (1994) Acta Cryst. C50, 655-656. Synthesis and structures of the partially ordered rock salt phases, Li3M2XO6: M = Mg, Co, Ni; X = Nb, Ta, Sb. Ma

cubic lithium niobium oxide

2001-05-25 Thread Diffract
could somebody direct me to the structure of cubic lithium niobium oxide (Li3NbO4 ao~8.4A); what is it isostructural with? L. Keller

Re: cubic lithium niobium oxide

2001-05-24 Thread Andreas Leineweber
[EMAIL PROTECTED] schrieb: > could somebody direct me to the structure of cubic lithium niobium oxide (Li3NbO4 >ao~8.4A); what is it isostructural with? > > L. Keller Results of a short cross-check with the ICSD database: Li3NbO4 is I-43m, cI64 K. Ukei et al. Acta Cryst C 50 (1