Re: conversion of rigaku data file

2015-02-11 Thread Roberto R. de Avillez
[mailto:rietveld_l-requ...@ill.fr] *On Behalf Of *Davide Levy *Sent:* Wednesday, 11 February 2015 1:50 AM *To:* rietveld_l@ill.fr *Subject:* conversion of rigaku data file Hi, do you know how convert rigaku data file (.raw or .asc) to an xy file? Thanks Davide

RE: conversion of rigaku data file

2015-02-10 Thread Ian.Madsen
[mailto:rietveld_l-requ...@ill.fr] On Behalf Of Davide Levy Sent: Wednesday, 11 February 2015 1:50 AM To: rietveld_l@ill.fr Subject: conversion of rigaku data file Hi, do you know how convert rigaku data file (.raw or .asc) to an xy file? Thanks Davide

Re: conversion of rigaku data file

2015-02-10 Thread Holger Kletti
Hello Davide, as Martin suggested, PowDLL definitely works. Holger Hi, do you know how convert rigaku data file (.raw or .asc) to an xy file? Thanks Davide <>++ Please do NOT attach files to the whole list Send commands to eg:

Re: conversion of rigaku data file

2015-02-10 Thread Martin Etter
Hi Davide, you can try to use PowDll: http://users.uoi.gr/nkourkou/powdll/ Best wishes, Martin Am 2/10/2015 3:50 PM, schrieb Davide Levy: Hi, do you know how convert rigaku data file (.raw or .asc) to an xy file? Thanks Davide

conversion of rigaku data file

2015-02-10 Thread Davide Levy
Hi, do you know how convert rigaku data file (.raw or .asc) to an xy file? Thanks Davide ++ Please do NOT attach files to the whole list Send commands to eg: HELP as the subject with no body text The Rietveld_L list archive is on