Re: Tricks for transmission sample preparation between foils

2017-02-10 Thread François Goutenoire
Thank every one for the propositions. Find here after the result of a test (vaseline + n-heptane) http://perso.univ-lemans.fr/~fgouten/Transmission_Tricks Best Regards, François Le 08/02/2017 13:35, François Goutenoire a écrit : Dear Rietveld users, We are currently using transmission flat s

Re: Tricks for transmission sample preparation between foils

2017-02-09 Thread Young, Lindsay Kay
2017 12:08:57 AM To: François Goutenoire; rietveld_l@ill.fr Subject: Re: Tricks for transmission sample preparation between foils Dear Pr. Francois GOUTENOIRE, In case of kapton tape there is a chance of getting diffraction peak at low angle, I prefer to use magic scotch tape. Some times to avoi

Re: Tricks for transmission sample preparation between foils

2017-02-08 Thread srihari velaga
  Dear Pr. Francois GOUTENOIRE, In case of kapton tape there is a chance of getting diffraction peak at low angle, I prefer to use magic scotch tape. Some times to avoid the background from this tape as well, I use small punch in the thick paper card and pack the material in that hole for transmi

RE: Tricks for transmission sample preparation between foils

2017-02-08 Thread gili cohen taguri
t the results? Thanks in advance, Gili -Original Message- From: rietveld_l-requ...@ill.fr [mailto:rietveld_l-requ...@ill.fr] On Behalf Of Fran?ois Goutenoire Sent: Wednesday, February 08, 2017 2:35 PM To: rietveld_l@ill.fr Subject: Tricks for transmission sample preparation between

Tricks for transmission sample preparation between foils

2017-02-08 Thread François Goutenoire
Dear Rietveld users, We are currently using transmission flat sample on our diffractometer. To prepare the transmission flat sample we are using mylar 15microns or kapton. We put the sample between 2 mylar foils. I would like to know if there is some tricks in order to nicely put the powder