Hi All,
I am trying to run a batch file in topas and I am getting the following error:
Abnormal program termination.
C:\Topas>tc.exe C:\Topas\Claire_RR_CIFs\._Pb\Pb_7_batch_rietveldrefinement
"macro uu {001} macro vv {120} macro ind {00120} "
TOPAS-64 Version 7.21 (c) 1992-2020 Alan A. Coelho
Hi Davide
I have come across that type of error before, but not in that context (I
think).
Are you able to share your input file/data? I can try on my topas and see
if it works.
Matthew
On Sun, 26 Jun 2022, 15:17 , wrote:
> Good morning,
>
> I have got a problem with Topas 5. When I try to lo
Good morning,
I have got a problem with Topas 5. When I try to load a .imp file with the
command Auto_T (10) to perform simulated annealing I receive this error message
:
access violation at address 78BA2313 in module 'TB_MFC-DLL.DLL'.
Does anybody know how to resolve this problem?
Thanks
Da