Re: Structure of silicon carbide

1999-02-04 Thread Diffract
Extensive review of SiC polytypes (incl. atomic positions) by P.T.B. Shaffer in Acta Cryst. B25, 477-488, 1969 l. Keller

Structure of silicon carbide

1999-02-04 Thread Hudgens, Bruce
I need the structure of SiC 3C (moissanite). If someone has the atomic positions and/or a journal reference, I would appreciate receiving it. Thanks in advance. Bruce A. Hudgens Research Associate USG Research & Technical Center 700 N Hwy 45 Libertyville, IL 60048 [EMAIL PROTECTED] (847) 970-506