Re: Structural refinement with variable divergence slit

1999-05-04 Thread Dr. R. Kleeberg
At 15:04 28.04.99 +0200, you wrote: >We would like to use the variable slit attached with our diffractometer for >Rietveld refinement. I have read the basic papers on the subject : Modern >Powder Diffraction + the paper by M.E.Bowden et al « Comparison of >intensities from fixed and variable div

Structural refinement with variable divergence slit

1999-04-28 Thread Francois Goutenoire
Hi all rietveld users, We would like to use the variable slit attached with our diffractometer for Rietveld refinement. I have read the basic papers on the subject : Modern Powder Diffraction + the paper by M.E.Bowden et al « Comparison of intensities from fixed and variable divergence X-ray di