Dear K. Suresh,
Metakaolin is formed when kaolinite is calcined losing water through
dehydroxilization (500 -800°C), wich produces an amorphous material. For
this razon you can not access the PDF or CIF of metakaolin.
Happy new year.
José A. Henao
> Dear Rietvelder,
>
>
>
> Can anyone of you se
Dear Rietvelder,
Can anyone of you send me the JCPDS number of metakaolin and its Cif. I have
difficulty to access these files. Many sincere thanks for this help & Happy
2010!!!.
Dr. K. Suresh