RE: GSAS data formats

2009-03-16 Thread Matthew.Rowles
Email: matthew.row...@csiro.au From: Brian H. Toby [mailto:brian.t...@anl.gov] Sent: Tuesday, 17 March 2009 00:31 To: vondre...@anl.gov Subject: Re: GSAS data formats I don't think this went to the mailing list On Mar 16, 2009, at 7:44 AM, Robert Von Dr

[Fwd: Re: GSAS data formats]

2009-03-16 Thread Robert Von Dreele
ele - Original Message - From: "Brian H. Toby" Date: Monday, March 16, 2009 0:30 am Subject: Re: GSAS data formats To: matthew.row...@csiro.au Cc: rietveld_l@ill.fr I do not recommend using this format. Better choices are the ESD variant on this, where numbers are alternated int

Re: GSAS data formats

2009-03-15 Thread Brian H. Toby
I do not recommend using this format. Better choices are the ESD variant on this, where numbers are alternated intensity, esd, intensity... (and there are a lot more digits for each number) or the FXYE format, which has angle, intensity, and optionally esd, one entry per line in free format