Perhaps I missed a followup to this during my absence, but if you don't find
the exact structure in ICSD, try looking for an isomorph eg in the case of
Cs2SiO3 you will find 9 possible isomorphs including Na2SiO3 if you search
for compounds with ANX formula AB2X3 containing Si1 and O3.
Let me kn
I could only find the structure parameters for Cs2Si2O5 in our reasonably
updated ICSD database. I wonder if there are any published structure data
out there. Good luck.
Tao
10/30/98
On Fri, 30 Oct 1998, Hongwu Xu wrote:
> Dear All:
>
> Does anyone have structural information (space grou