Re: Generator for Scintag

2004-07-19 Thread Andrew Wills
Dear Qisheng, I just wanted to remind people interested in magnetic rietveld studies of the programs that perform magnetic symmetry analysis, such as SARAh (ftp.ill.fr/pub/dif/sarah) and BasiReps (included in the FullProf Suite). These programs work out different 'symmetry-allowed' magnetic struc

RE: Generator for Scintag

2004-07-15 Thread Qisheng Lin
Dear all, I am a newer in magnetic structure determination. I am trying to refining a magnetic structure of double perovskite containing Mn2+ and Mo5+, the nuclear structure is crystallized in P21/n, with Mn (1/2 0 1/2) and W (0 1/2 0). The propagation vector for magnetic cell is (1/2 1/2 0). Can

RE: Generator for Scintag

2004-07-15 Thread Frank, Steven
Peter, I received your first message, sorry no generator here. Have you tried Karl Hofmann at Compass Engineering ([EMAIL PROTECTED])? Good Luck. Steve Frank ANL-W -Original Message- From: Peter Zavalij [mailto:[EMAIL PROTECTED] Sent: Thursday, July 15, 2004 2:11 PM To: Mailing List,

RE: Generator for Scintag

2004-07-15 Thread Peter Zavalij
Hi everyone, Sorry for asking again but I am not sure I send this message first time. I am looking for an old/used generator for Scintag XDS2000 diffractometer. New one is too expensive as for old machine. Any suggestions/contacts are welcome. Thanks in advance, Peter Zavalij University Cryst