>> I didn´t find the crystalline phase
>> K_6 H_2 Nb_6 O_19 .8H_2 O
>> in ICSD database
>
> K7(H Nb6O19).(H2O)10 which is already pretty close,
I should have given the reference for this and other similar Nb6O19
cluster compounds as:
"Solid-state structures and solution behavior of alkali salts o
> I didn´t find the crystalline phase
> K_6 H_2 Nb_6 O_19 .8H_2 O
> in ICSD database
There are very many phases containing niobium oxide blocks, with various
other cations and hydration states, so you may not find an exact match.
You can still use ICSD to help understand the structure if you rela
Dear Rietveld´s users,
I didn´t find the crystalline phase
K_6 H_2 Nb_6 O_19 .8H_2 O
in ICSD database, if you know how to get crystallographic data, please
let me know.
Many thanks in advance
Sasaki
--
_
Dr. Jose Marcos Sasaki (professor associado