Re: CIF for Pyrrhotite 4C

2007-02-03 Thread Alan Hewat
> Can anyone help me with a CIF file for Pyrrhotite 4C. The CIF output > from ICSD #42491 gives SG 15 setting F12/d1 which is not recognized by > TOPAS. ICSD http://icsdweb.fiz-karlsruhe.de/ also gives a more recent entry for Fe7S8 Pyrrhotite 4C in setting C12/c1 (if you have access to the full d

RE: CIF for Pyrrhotite 4C

2007-02-02 Thread AlanCoelho
. cheers alan -Original Message- From: Allen, Douglas R. [mailto:[EMAIL PROTECTED] Sent: Saturday, 3 February 2007 8:02 AM To: rietveld_l@ill.fr Subject: CIF for Pyrrhotite 4C Can anyone help me with a CIF file for Pyrrhotite 4C. The CIF output from ICSD #42491 gives SG 15 setting F12/d1

CIF for Pyrrhotite 4C

2007-02-02 Thread Allen, Douglas R.
Can anyone help me with a CIF file for Pyrrhotite 4C. The CIF output from ICSD #42491 gives SG 15 setting F12/d1 which is not recognized by TOPAS. I found an entry in the ICDD database from the Linus Pauling file which shows the setting A12/A1 but when the CIF file is exported the same unrecogni