would give a peak, if all are oriented
to same direction.
Thats my thoughts, please correct me if Im totally mistaken with this.
BR,
Mikko
From: Angel L. Ortiz [mailto:alor...@unex.es]
Sent: 25. lokakuuta 2013 11:19
To: 'Mikko Heikkilä'; Rietveld_l@ill.fr
Subject: roc
literature but no
success so far. Hopefully you can make me feel stupid and find out the easy
solution before I do J
Have a nice weekend!
BR,
Mikko
---
Mikko Heikkilä, M.Sc., Laboratory engineer
Laboratory of Inorganic Chemistry
Department of Chemistry
P.O. Box 55 (A.I. Virtasen
ions for
> calibrants? My only serious worry is whether there is any potential
> for ceria to react with, the Pt strip?
> (Perhaps under vacuum?) I'd welcome any advice or suggestions.
> Yours
> Rory
>
> *****
x27;t really
matter. Anyway, I'd be more than happy if someone here would know the
reason for this phenomenon.
Regards,
Mikko
--
Mikko Heikkilä, M.Sc.
Laboratory of Inorganic Chemistry
Department of Chemistry
P.O.Box 55 (A.I. Virtasen aukio 1)
FI-00014 University of Helsinki
Eduard E. Le
Prof. Agr
>> (Assoc. Prof.) de Física Tel: (+598 2) 9290648/9249859
>> Cryssmat-Lab./DETEMA Fax: (+598 2) 9241906
>> Facultad de Quimica, Universidad de la Republica
>> ,_.
>> | \
>> | v-
>> ,' \
>>
don't have any experience with ovens from other manufacturers, but
this combination seems to work very well.
Best regards,
Mikko
--
Mikko Heikkilä, M.Sc
Laboratory of Inorganic Chemistry
Department of Chemistry
P.O.Box 55 (A.I. Virtasen aukio 1)
FI-00014 University of Helsinki
r.m.
o read this through.
Best regards and successfull start to your year,
Mikko
---
Mikko Heikkilä, M.Sc.
Laboratory of Inorganic Chemistry
Department of Chemistry
P.O.Box 55
FI-00014 University of Helsinki
phone: +358 9 191 50216
mobile: +358 440 572 372
email: mikko.j.heikk...@helsinki.fi