You
should multiply all of the crystalline phases by 5/7 with the remaining 2/7
being your amorphous phases.
-Original Message-From: Ferdinando Costantino
[mailto:[EMAIL PROTECTED]]Sent: Friday, June 15, 2001 9:32
AMTo: [EMAIL PROTECTED]Subject: internal standard for
glass
Title: Natrite - Na2 CO3
Does anyone have the structural coordinates for sodium carbonate? I will be greatful if you could send them to me. Thanks in advance.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
Libertyville, IL 60048
(847) 970-5064 (voice)
(847) 970-5299 (fax)
Title: Tricalcium aluminate
I need the orthorhombic structure for tricalcium aluminate (C3A). Thanks in advance.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
Libertyville, IL 60048
(847) 970-5064 (voice)
(847) 970-5299 (fax)
Title: Structure of Gorgeyite
If anyone could provide me with the crystal structure data and/or journal reference, it will help me greatly. Thanks in advance.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
Libertyville, IL 60048
(847) 970-5064 (voice)
(847) 970-5299 (fax)
Title: Calcium iron titanium oxide
If anyone can provide the atomic positions and/or a reference for the structure Ca3 Fe2 Ti O8, it will help me greatly. I am attempting analyze high aluminate cement. Thank you for your help.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
L
Title: Structures of katoite, katoite-silication, and calcium sulfate monosulfate
Does anyone have references and/or coordinates for katoite, Ca3 Al2 (OH)12, katoite-silication, Ca3 Al2 (SiO4) (OH)8 and calcium sulfate monosulfate, Ca4 Al2 O6 (SO4) 12H2O. Any help that can be provided will gr
Could someone provide me with a reference and/or atomic coordinates for
archerite (ICDD 34-807)? Any help will greatly appreciated.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
Libertyville, IL 60048
(847) 970-5064 (voice)
(847) 970-5299 (fax)
Does anyone have a reference for the structure of KMgPO4 * 6H2O (ICDD card
35-0812)? Any help will be greatly appreciated.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
Libertyville, IL 60048
(847) 970-5064 (voice)
(847) 970-5299 (fax)
Does anyone have references to the structures of tobermorite,
Ca5Si6(O,OH,F)18_5H2O, and/or rapidcreekite, Ca2(CO3)SO4_4H2O? Any
information will be greatly appreciated.
Bruce A. Hudgens
USG Research & Technical Center
700 N. Hwy 45
Libertyville, IL 60048
(847) 970-5064 (voice)
(847) 970-5299
Can anyone provide me with the coordinates and/or a reference for the
structure of yeelimite, Ca4 Al6 O12 SO4? Thanks in advance for your help.
Bruce Hudgens
USG Corporation
700 N Hwy 45
Libertyville, IL 60048
[EMAIL PROTECTED]
Does anyone have a reference for the crystal structure of stratlingite?
Stratlingite = Ca2 Al2 Si O7 - 8H2O
Any help locating the structure and/or reference will be greatly
appreciated. Thanks.
Bruce A. Hudgens
USG Research & Technology Center
700 N Hwy 45
Libertyville, IL 60048
[EMAIL PROTECT
I need the structure of SiC 3C (moissanite). If someone has the atomic
positions and/or a journal reference, I would appreciate receiving it.
Thanks in advance.
Bruce A. Hudgens
Research Associate
USG Research & Technical Center
700 N Hwy 45
Libertyville, IL 60048
[EMAIL PROTECTED]
(847) 970-506
x y z B
Zr 0 0 0 1.66
O 0 .5 .1853.11
a 3.64
b 3.64
c 5.27
Bruce A. Hudgens
Research Associate
USG Research & Technical Center
700 N Hwy 45
Libertyville, IL 60048
[EMAIL PROTECTED]
(847) 970-5064 Voice