Re: XRDML to RD or RAW

2008-02-04 Thread Gregory A Stephenson
You might want to look at this crivetz <[EMAIL PROTECTED] m>

Re: crystallite size determination

1999-05-19 Thread Gregory A Stephenson
How does one handle the problem of bimodal particle size distributions by diffraction techniques? My previous experience at particle size measurements using laser light scattering indicates non-monomodality is the norm rather than the exception. Can powder diffraction resolve this?

Re: Question

1998-11-11 Thread Gregory A Stephenson
Frank McClune at the International Centre for Diffraction Data 12 Campus Boulevard Newtown Square, Pennsylvania 19073-3273 U.S.A. More info at: www.icdd.com Sincerely, Greg Stephenson