Hi Jan
Independent Minerals Standards have a corundum certified at 99.04%
crystalline. It was done* via external standard calibration by reference to
NIST 676a.
https://imstandards.com.au/independent-mineral-standards-releases-ims135/
*I was involved in the XRD measurements that were used in th
Just a reminder - SNS and HFIR are currently accepting General User proposals
for cycle 2025-A. The deadline is coming up on Wednesday, August 28. Proposals
awarded beam time at SNS are projected to run January 28 to May 27, 2025.
Details about instrument participation and conditions are provid
Dear All,
SRM 676 (corundum for QPA) at NIST has been out of stock for some time. Is
there an alternative supplier for some similar standard(s)?
Thank you in advance,
Jan Rohlicek
Institute of Physics CAS
Cukrovarnicka 10/112
162 00 Prague 6
Tel: (+420) 220 318 484