Hi all
I've been trying to find a good explanation of what parafocussing (wrt
Bragg-Brentato geometry) actually is, but haven't been able to find one.
Klug and Alexander just reference Brentano's papers.
"The Basics of Crystallography and Diffraction" 2nd ed say that B-B
geometry is "semi-focuss
Dear Colleagues,
Sorry for this not strictly -Rietveld related- question.
Could anyone suggest a free software to generate jpg or tiff files of 3D
views, from different perspectives, of multiple powder patterns collected
in in-situ XRPD measurements vs T or t. A colleague not very used to powder