Dear Colleagues,
just to inform you: The BGMN Rietveld program is now available for the
Mac too. Pricing for the full/academic licence will be similar to the
Windwos/Linux versions, a demo is available at www.bgmn.de.
Regards
Joerg Bergmann
Dear All,
Could you please advice if you have the literatures on Applications of XRD/XRF
in the oil industry.
Thank in advance for your help.
Yours sincerely, and best wishes
Husin
Quoting Nicolae Popa <[EMAIL PROTECTED]>:
> Hi,
>
> Besides strain and instrument also size broadening can be cl