RE: La336

2001-03-27 Thread Peter Y. Zavalij
It is the closest much to your compound: La1.5Ba1.5Cu3O7.2 Izumi et al. Japan. J. Appl. Phys., Part 2. 27 (1988) L824-L826. -Original Message- From: S. Nagesh Kini [mailto:[EMAIL PROTECTED]] Sent: Tuesday, March 27, 2001 8:45 PM To: [EMAIL PROTECTED] Subject: La336 I am looking for a

La336

2001-03-27 Thread S. Nagesh Kini
I am looking for a refence on neutron diffraction study of La3Ba3Cu6O14. Could anybody help me? Thanks -Kini

GSAS question

2001-03-27 Thread Sang-Heon Shim
Dear Expert, I want to plot background subtracted calculated and observed histogram data using other softwares (e.g., IGOR). hstdmp gives me 0's in background column (I probably did something wrong). Would you let me know how I can get background subtracted histogram dat