RETRIEVE

2000-11-23 Thread Yasuhiro TAKAHASHI
Is there anybody who installed the Inorganic Crystal Structure Data Base on a Windows ME? The RETRIEVE program gives me an run time error. thank you Davide Levy ATTENTION! DO NOT USE CAPITAL LETTERS IN MY E-MAIL ADDRESS ATTENZIONE! NON USARE LETTERE MAIUSCOLE NEL MIO INDIRIZZO E-MAIL ___

RE: TiB2 crystal structure

2000-11-23 Thread Peter Y. Zavalij
To my recollection it is AlB2 structure type: sp.gr. P6/mmm, a=3 A, c=3.2 A Al in 0,0,0 B in 1/3,2/3,1/2 Peter Zavalij -Original Message- From: Anthony Manerbino [mailto:[EMAIL PROTECTED]] Sent: Thursday, November 23, 2000 11:54 AM To: '[EMAIL PROTECTED]' Subject: TiB2 crystal structure

TiB2 crystal structure

2000-11-23 Thread Anthony Manerbino
Dear Rietveld list subscribers, Does anyone know where I could find a publication with any information on the structure of TiB2? Cheers, Anthony Manerbino