I enjoyed Mr. Woods' comments. Years ago when Resorcinol was the FAA standard for aircraft wood glues I came up with a formula that was widely used until 1:1 ratio T88 came on the scene. Hughes in Detroit worked with me to come up with FPL 16A. Essentially formula FPL 16 (Forest Products La

KR> thinning epoxy (Hughes Glue)

2008-10-12 Thread Larry&Sallie Flesner
At 03:23 PM 5/21/2007, you wrote: >Hughes in Detroit worked with me to come up with FPL 16A. > Essentially formula FPL 16 (Forest Products Laboratory) was modified >by addition of more MEK to improve penetration. The end ratio was 10:1. >The whole story was reported in Sport Aviation in the Octo

KR> thinning epoxy (Hughes Glue)

2008-10-12 Thread Sid Jongsma
Hi Mick I spoke with you several times about HUGHES GLUE when I began an all wood CA65 airplane project: about 20 years ago. (wher did the time go? I found to be a wonderful glue I is still my favorite glue and is relativly easy to use if you are careful . . >I enjoyed Mr. Woods' comments. >