In a message dated 05/19/2000 12:53:29 PM Pacific Daylight Time, 
[EMAIL PROTECTED] writes:

<< Can anyone recommend literature references for
 size/strain analysis on "organic" (C, H, O, N)  
 phases?  >>

Do you include polymers which are organic? Then the treatments by Hosemann or 
Ruland may be for you. All 1950-60's work with good introductions to be found 
in the Alexander classic "X-Ray Diffraction Methods in Polymer Science". 

L. Keller