At 10:14 19/11/1999 +0100, you wrote:
>Thanks to all for sending me the informations.... and sorry; I should find
>by myself the BaSiF6 structure in ICSD, but in reality I look in there for
>the CaSiF6 or similar structure (ABX6 and tetragonal), so I miss the BaSiF6
This is a common error when searching ICSD, so no need to apologise :-)
Many people over-restrict their search by specifying too many conditions.
In general you should avoid assuming you know the symmetry, or worse the
space group.
Searching on just ABX6 with 3 elements will give only 157 results, a small
enough number to look at; almost all are halides and most are rhombohedral,
with only a handful tetragonal.
Alan.
Alan Hewat, ILL Grenoble, FRANCE <[EMAIL PROTECTED]> tel (33) 4.76.20.72.13
ftp://ftp.ill.fr/pub/dif fax (33) 4.76.20.76.48 http://www.ill.fr/dif/