Hi Mark. John Shaffer here. On my first KR exhaust, I used Hi-temp,
1200 or 1500 , header paint. Next one I had Electroless Nickel plated
( external only) and it made about 8 years. My present is Jet-Hot
coated silver, and is coated inside and outside. It has been in
service just under 2 years, with no apparent degradation.


-- 