After that Rand recommended Safe-T-Poxy which is today called EZ Poxy. I still use the EZ poxy. Seems most people use West or Aeropoxy, but I have used them all and find the EZ far superior. Wrote a long post about the reasons why a long time ago and I suppose it could be dug up in the archives.
Brian Kraut 904-536-1780 br...@eamanuacturing.com -------- Original Message -------- Subject: Re: KR> Rand Robinson's early epoxy (was Wing Attach Fittings) From: Mark Langford via KRnet <krnet@list.krnet.org> Date: Thu, April 06, 2017 7:33 am To: "KRnet" <krnet@list.krnet.org> Cc: m...@n56ml.com >From one of the Newsletters: RR epoxy is Shell Epon 813 resin, and General Mills Versamid 125 hardener. The first time I used this, my arms looked like I'd been burned in a house fire, so beware... _______________________________________________ Search the KRnet Archives at https://www.mail-archive.com/krnet@list.krnet.org/. Please see LIST RULES and KRnet info at http://www.krnet.org/info.html. see http://list.krnet.org/mailman/listinfo/krnet_list.krnet.org to change options. To UNsubscribe from KRnet, send a message to krnet-le...@list.krnet.org