I have been using Dap 00204 Plastic Resin Glue. Same issues with temp and clamping you indicated so I don't think it's any better or worse. I will use T88 for little bit of the structural stuff I have left to do.
Craig www.kr2seafury.com Corvair 2780cc --- On Thu, 8/18/11, Patrick and Robin Russo <patru...@myfairpoint.net> wrote: > From: Patrick and Robin Russo <patru...@myfairpoint.net> > Subject: Re: KR> Resorcinol Glue > To: "KRnet" <kr...@mylist.net> > Date: Thursday, August 18, 2011, 4:17 PM > I have 50 years of woodworking > experience and have always been less than > pleased with Resorcinal glues. If it's not clamping > pressure then it is > consistency, working time, shop temperature, shelf life, > etc.,etc. It is not > a forgiving glue. Alternatives...??? T-88..??? difficult to > do larges > assemblies, good gap filler but if its filling a gap you > have a bad > (brittle) joint, also need more than moderate clamping > pressure.