All,
Thanks for the respons, 
There is one misunderstanding. I am planning to go for 3 or 5 layers CF and not 
for Cres steel Phil Matheson have the cres steel one. The core of the barr will 
be foam.
We will start with 3 layers of CF en will put maybe  later some more based on 
the stengt of the 3 layers. Again if you all say 3 layers is to many I will 
start with 5

Thanks Stef




Stef and Ted are building the KR-2S     see   
http://www.masttotaalconcept.nl/kr2



________________________________

Van: krnet-boun...@mylist.net namens stef...@kpnmail.nl
Verzonden: do 10-2-2011 10:52
Aan: kr net
Onderwerp: KR> roll barr



KR friends,

We are starting to make our roll barr. We made it from the normal foam ( wings) 
and will wrap it around with cf
210 gr sq meter.
What are your fealings about how many layers I need for a save produkt.
The bar is about 3 x 3 inch. I am  planning for 3 layers or should I take 4 or 
5 or 6???

Thanks
Stef





Stef and Ted are building the KR-2S     see   
http://www.masttotaalconcept.nl/kr2


_______________________________________
Search the KRnet Archives at http://www.maddyhome.com/krsrch/index.jsp
to UNsubscribe from KRnet, send a message to krnet-le...@mylist.net
please see other KRnet info at http://www.krnet.org/info.html

Reply via email to