I have stayed out of the West System discussion -- But , I had tried
some samples for wood and was not happy with the results. I have used the
West System for all glass on 357CJ. I liked using the pumps for the
mixture it wet out glass as well as carbon fiber just fine. I used it for
all flox and micro also. It sands well and does not gum up the sand
paper.
Only my opinions from experience and a flying plane.
Joe Horton
On Fri, 27 Jan 2006 17:40:22 EST bdazzca...@aol.com writes:
> Hi Netters,
>
> Ok so I have figured out that I am going to go with the T-88
> for
> strucual epoxy...but what about for composite epoxies? Who's using
> what? What's
> best? Poly Poxy was brought up. As far as spar length....I plan on
> using the 5048
> airfoil for the inner spars.... someone was saying maybe if I
> wrapped them in
> CF that it might work. Any Advise on that idea?
>
>
>
> David Swanson
> bdazzca...@aol.com
> _______________________________________
> Search the KRnet Archives at
> http://www.maddyhome.com/krsrch/index.jsp
> to UNsubscribe from KRnet, send a message to krnet-le...@mylist.net
> please see other KRnet info at http://www.krnet.org/info.html
>
>