Well said Orma
But also I find when first mixing the West System I sit the container into
hot water to heat the mixed resin , this starts off the setting process,
just as using it in hot weather,
Caution, drying in the sun can cause air bubbles to swell

The gluing lost time is the pitts,
SO you need other items item the go all the time, so when you have finished
gluing. you can carry on with another part of the KR construction, and we
all know there are plenty of parts to make.