I have been doing a little glass work on my canopy ( see pics).  The
outside temp was in the low 30s...around 40 in the garage.  I have an oil
filled electric radiator that will bring the temp in the garage to close to
50.  I use US composite medium pot life resin...usually cures in about 8
hours.  The other night I did the radiator trick for about 10 hours...then
before I went to bed I used a heat gun to raise the temp to 150 and held it
there for a few minutes...then shut everything off.  Even though the temp
was freezing overnight it was cured by morning.  The heat gun works OK for
small areas but I wouldn't recommend it for large areas.

https://sites.google.com/site/mykr2stretch/
https://sites.google.com/site/mykr2stretch/parts-for-sale
On Jan 3, 2015 1:40 AM, "Dubi Gefen via KRnet" <krnet at list.krnet.org> wrote:

> Hello Friend
>
>
>
> I am preparing my aircraft to painting so now I am glassing the surface
> area
> of the wings and also the fuselage.
>
> My problem is the temperature of environment.
>
> The temperature in Israel drop down less than 53F and the glass is not
> getting hard.
>
>
>
> Could you suggest other type of epoxy?
>
> Now I am using PR2032 Aeropoxy
>
>
>
> Best regards Dubi Gefen
>
>  <mailto:Dubi_g at maanit.org.il> Dubi_g at maanit.org.il
>
>  <http://www.dubigefen.50megs.com/> http://www.dubigefen.50megs.com/
>
> +972-54-4921263
>
>
>
>
> This mail was sent via Mail-SeCure System.
>
>
> _______________________________________________
> Search the KRnet Archives at http://tugantek.com/archmailv2-kr/search.
> To UNsubscribe from KRnet, send a message to KRnet-leave at list.krnet.org
> please see other KRnet info at http://www.krnet.org/info.html
> see http://list.krnet.org/mailman/listinfo/krnet_list.krnet.org to change
> options
>

Reply via email to